Rcv'd today Stazi, appreciate your offer, time and efforts.
Tnx and now to get them all installed properly. Warmer weather
got to get the rotors cold galvinized Rust-Oleum's Since you guys have found these rotors/along with these pads less prone to warping. Want to keep rust to a minimum.

1.7785 Galvanizing compound (used as a primer on new steel)---I even spayed this on rusty exhaust pipes, but as soon as the salt/miosture gets on the pipes, the galvanic action/corrosion starts and the zinc in the coating becomes the sacrificial element and you have to re-coat in the spring. It's all about slowing down the process, we can't stop it.
2.7584 Cold galvanizing compound very heavy zinc. For those who live in non salted roads you could stop here, if you want the silver look. It's easily touched up.
3. 7716 Heat resistant silver for the Top coat.
Care taken to minimize paint on the wear area.

This Ole Fart hates winter salt Hi Hi
Take Care
Paul


Paul 98 Mystique LS 2ea (07/97)(08/98)